Interlaminar fracture properties of carbon fibre/epoxy matrix composites interleaved with polyethylene terephthalate (PET) films
Autore:
Jiang, W; Tjong, SC; Chu, PK; Li, RKY; Kim, JK; Mai, YW;
Indirizzi:
City Univ Hong Kong, Dept Phys & Mat Sci, Kowloon, Hong Kong, Peoples R China City Univ Hong Kong Kowloon Hong Kong Peoples R China g, Peoples R China Hong Kong Univ Sci & Technol, Dept Mech Engn, Kowloon, Hong Kong, Peoples R China Hong Kong Univ Sci & Technol Kowloon Hong Kong Peoples R China s R China City Univ Hong Kong, Dept Mfg Engn & Engn Management, Kowloon, Hong Kong, Peoples R China City Univ Hong Kong Kowloon Hong Kong Peoples R China g, Peoples R China
Titolo Testata:
POLYMERS & POLYMER COMPOSITES
fascicolo: 2, volume: 9, anno: 2001,
pagine: 141 - 145
SICI:
0967-3911(2001)9:2<141:IFPOCF>2.0.ZU;2-9
Fonte:
ISI
Lingua:
ENG
Soggetto:
GRAPHITE EPOXY; TOUGHNESS; CFRP; THICKNESS; ADHESION;
Tipo documento:
Article
Natura:
Periodico
Settore Disciplinare:
Engineering, Computing & Technology
Citazioni:
16
Recensione:
Indirizzi per estratti:
Indirizzo: Li, RKY City Univ Hong Kong, Dept Phys & Mat Sci, Tat Chee Ave, Kowloon, Hong Kong, Peoples R China City Univ Hong Kong Tat Chee Ave Kowloon Hong Kong Peoples R China
Citazione:
W. Jiang et al., "Interlaminar fracture properties of carbon fibre/epoxy matrix composites interleaved with polyethylene terephthalate (PET) films", POLYM POL C, 9(2), 2001, pp. 141-145

Abstract

A study has been made of the interlaminar fracture behaviour of unidirectional carbon fibre-epoxy matrix composites containing polyethylene terephthalate (PET) interleaving films,with and without plasma surface treatment. Comparisons are made of the initiation Values of mode I and mode II interlaminar fracture toughness, G(Ic) and G(IIc), for composites with and without interleaves. It is shown that the interleaves have completely reverse effects on interlaminar fracture toughness with different mo des of fracture. Theinterleaves have the detrimental effect of reducing G(Ic), up to 70%, and the plasma treatment is effective in mitigating the toughness reduction. Insharp contrast, the interleaves improve the corresponding toughness in mode II, with a negligible influence of plasma treatment on G(IIc). The major failure mechanisms associated with the presence of interleaves are discussed.